Yellow Gold Alloy for mechanical work 18K 2N B182N per gram
Additive for making 18K yellow gold.
technical-sheet
Suitable for mechanical work.
Best choice for solid and hollow products.
Best choice for solid and hollow products.
High chemical resistance.
High gloss level.
2N colour: light yellow.
2N colour: light yellow.
Melting temperature: 995-1065°C
Per gram